Select black pigment for masterbatch according to the carrier polymer and final application. A grade that works in an injection-moulded part may behave differently in thin film or fibres.
Define the production requirements
- Carrier resin, such as PE or PP, and resin specifications
- Pigment concentration in the masterbatch and masterbatch dosage in the final product
- End use: film, moulded parts, pipes or fibres
- Extruder, mixing conditions and filtration constraints
Compare samples under controlled conditions
Use the same resin, additives, dosage and processing conditions for the reference and candidate pigment. First compare equal dosages; then separately adjust dosage to reach the target colour. Record both results.
What to record
Compare colour and undertone on samples of equal thickness. Record surface specks, coarse particles, dispersion, torque, pressure, filter behaviour and output stability. Evaluate colouring cost at the dosage needed to meet the quality target, rather than comparing price per kilogram alone.
Why do black specks appear?
Agglomeration, insufficient mixing, contamination and unsuitable processing can contribute. Check equipment cleanliness, feed sequence, mixing and carrier compatibility before attributing the problem to the pigment grade.
How much pigment is needed?
There is no universal dosage for every polymer and end use. Determine it through trials for colour, dispersion, final properties and processability. Distinguish masterbatch dosage from pigment concentration.
Request technical advice and samples
Send the polymer, final product, current grade, dosage, observed problem and monthly consumption. Compare Gohar grades against their data sheets and production trials. Conductivity and weather resistance require separate verification in the final compound.